Here's the scenario, I have a 5' x 12' x 1 3/4" solid mahogany table top that is finished with 3 coats of Sherwin Williams Super Kemvar "m" conversion varnish. The varnish has set for 2 days and sanded from 800 titan 2 through Platin II 2000. The surface is nice and smooth but a little cloudy. The question is, what would be the best way to complete this process. Wax? just a felt pad to buff?