From what I have read, EM6500 is supposed to be well suited to spraying. But looking at the viscosity, it looks like it works out to something around 100 seconds on the Ford #4 cup.
I assume it needs to be thinned with some water.. but how far? Should I be trying to get it down to 20-25 seconds through a Ford #4? Are there any other reference points I can use as a starting place?
I'm planning to use a 1.8 aircap, which is what Target Coatings recommends for the product. Should I try a 1.5 or 1.3?
HVLP is pretty new to me, but I'm enjoying it so far and looking forward to improving at it.
Thanks,
Adam
I assume it needs to be thinned with some water.. but how far? Should I be trying to get it down to 20-25 seconds through a Ford #4? Are there any other reference points I can use as a starting place?
I'm planning to use a 1.8 aircap, which is what Target Coatings recommends for the product. Should I try a 1.5 or 1.3?
HVLP is pretty new to me, but I'm enjoying it so far and looking forward to improving at it.
Thanks,
Adam